Nedenfor presenterer vi klare, klare-til-brukhastelloy C276vekt- og prisdiagrammer basert på legeringens offisielle tetthet på 8,89 g/cm³ og gjeldende 2026 markedsforhold.

Hastelloy C276 tallerkenvekttabell
Vekten er beregnet ved å bruke legeringens tetthet på 8,89 g/cm³ (0,321 lb/in³). Den enkle formelen er:
Vekt (kg/m²)=platetykkelse (mm) × 8,89
Tabell 1: Hastelloy C276 platevekt etter tykkelse
|
Tykkelse (mm) |
Tykkelse (tommer) |
Vekt per m² (kg) |
Vekt per fot² (lbs) |
|
3,0 mm |
0.118" |
26,67 kg |
5,46 lbs |
|
5,0 mm |
0.197" |
44,45 kg |
9,10 lbs |
|
6,0 mm |
0.236" |
53,34 kg |
10,92 lbs |
|
8,0 mm |
0.315" |
71,12 kg |
14,56 lbs |
|
10,0 mm |
0.394" |
88,90 kg |
18,20 lbs |
|
12,0 mm |
0.472" |
106,68 kg |
21,84 lbs |
|
15,0 mm |
0.591" |
133,35 kg |
27,30 lbs |
|
20,0 mm |
0.787" |
177,80 kg |
36,40 lbs |
|
25,0 mm |
0.984" |
222,25 kg |
45,50 lbs |
|
30,0 mm |
1.181" |
266,70 kg |
54,60 lbs |
|
40,0 mm |
1.575" |
355,60 kg |
72,80 lbs |
|
50,0 mm |
1.969" |
444,50 kg |
91,00 lbs |
Her er faktiske vektberegninger for standard platestørrelser:
|
Platestørrelse (mm) |
Tykkelse |
Vekt per tallerken (kg) |
Vekt per tallerken (lbs) |
|
1000 × 2000 mm |
6 mm |
106,68 kg |
235,2 lbs |
|
1000 × 2000 mm |
10 mm |
177,80 kg |
392,0 lbs |
|
1000 × 2000 mm |
20 mm |
355,60 kg |
784,0 lbs |
|
1200 × 2400 mm |
6 mm |
153,62 kg |
338,7 lbs |
|
1200 × 2400 mm |
10 mm |
256,03 kg |
564,5 lbs |
|
1200 × 2400 mm |
20 mm |
512,06 kg |
1129,0 lbs |
|
1500 × 3000 mm |
10 mm |
400,05 kg |
882,0 lbs |
|
1500 × 3000 mm |
20 mm |
800,10 kg |
1764,0 pund |
|
2000 × 6000 mm |
15 mm |
1.600,20 kg |
3 528,0 lbs |
|
2000 × 6000 mm |
25 mm |
2.667,00 kg |
5 880,0 lbs |
Merknader: Verdiene er teoretiske; faktisk levert vekt kan variere med ±2 % på grunn av produksjonstoleranser.
Disse vektene hjelper deg raskt å beregne total belastning for trykkbeholdere, skrubbere eller varmevekslere. For egendefinerte størrelser multipliserer du bare kg/m²-verdien med ønsket område.
Hastelloy C276 Plate Prisguide
Prisene for Hastelloy C276-plater avhenger av tykkelse, mengde, finish (varmt- eller kaldvalset-) og gjeldende nikkel/molybden-markedsnivåer. Som en direkte produsent med vårt eget smelte- og valseanlegg, tilbyr vi konkurransedyktige fabrikk-direkte priser uten mellommann-påslag.
Tabellen nedenfor viser typiske 2026-leverte priser for standard ASTM B575 / ASME SB575 plater i mengder på 500 kg eller mer.
Tabell 2: Veiledende Hastelloy C276-platepris (USD/kg, FOB Kina)
|
Tykkelse (mm) |
Pris per kg (USD) |
Pris per lb (USD) |
Pris per m² (USD) |
|
3,0 mm |
$45 - $55 |
$20 - $25 |
$1,200 - $1,460 |
|
5,0 mm |
$42 - $52 |
$19 - $23.50 |
$1,867 - $2,311 |
|
6,0 mm |
$40 - $50 |
$18 - $22.50 |
$2,134 - $2,667 |
|
8,0 mm |
$38 - $48 |
$17 - $21.50 |
$2,703 - $3,414 |
|
10,0 mm |
$36 - $46 |
$16 - $20.50 |
$3,200 - $4,089 |
|
12,0 mm |
$35 - $45 |
$15.50 - $20 |
$3,734 - $4,801 |
|
15,0 mm |
$34 - $44 |
$15 - $19.50 |
$4,534 - $5,867 |
|
20,0 mm |
$33 - $43 |
$14.50 - $19 |
$5,867 - $7,645 |
|
25,0 mm |
$32 - $42 |
$14 - $18.50 |
$7,112 - $9,334 |
|
30,0 mm |
$31 - $41 |
$13.50 - $18 |
$8,268 - $10,935 |
|
40,0 mm |
$30 - $40 |
$13 - $17.50 |
$10,668 - $14,224 |
|
50,0 mm |
$29 - $39 |
$12.50 - $17 |
$12,891 - $17,336 |
Merk: Prisene som vises er veiledende intervaller basert på 2025-2026 markedsforhold.
Komplette tallerkenpriseksempler
Her er estimerte priser for komplette standardplater:
|
Tallerkenstørrelse |
Tykkelse |
Vekt |
Anslått pris (USD) |
|
1000 × 2000 mm |
6 mm |
107 kg |
$4,280 - $5,350 |
|
1000 × 2000 mm |
10 mm |
178 kg |
$6,408 - $8,188 |
|
1000 × 2000 mm |
20 mm |
356 kg |
$11,748 - $15,308 |
|
1200 × 2400 mm |
10 mm |
256 kg |
$9,216 - $11,776 |
|
1200 × 2400 mm |
20 mm |
512 kg |
$16,896 - $22,016 |
|
1500 × 3000 mm |
10 mm |
400 kg |
$14,400 - $18,400 |
|
1500 × 3000 mm |
20 mm |
800 kg |
$26,400 - $34,400 |
|
2000 × 6000 mm |
15 mm |
1.600 kg |
$54,400 - $70,400 |
|
2000 × 6000 mm |
25 mm |
2.667 kg |
$85,344 - $111,994 |
PrissammenligningAnnenMaterialer
Å forstå hvordan Hastelloy C276 kan sammenlignes med andre legeringer hjelper til med å rettferdiggjøre investeringen:
|
Materiale |
Pris per kg (USD) |
Relativ kostnad |
|
Rustfritt stål 316L |
$4 - $6 |
1x (grunnlinje) |
|
Tosidig 2205 |
$8 - $12 |
2x |
|
Legering 904L |
$15 - $20 |
3-4x |
|
Hastelloy C276 |
$30 - $50 |
7-10x |
|
Titan klasse 2 |
$25 - $35 |
6-8x |
|
Inconel 625 |
$45 - $65 |
10-12x |
Mens Hastelloy C276 koster mer på forhånd, resulterer dens overlegne korrosjonsmotstand ofte i lavere totale eierkostnader gjennom forlenget levetid og redusert vedlikehold.
Konklusjon
Å forstå Hastelloy C276 platevekt og prissetting er avgjørende for nøyaktig prosjektbudsjettering og materialvalg.
Vårt produksjonsanlegg opprettholder et omfattende lager av Hastelloy C276-plater med konkurransedyktige priser, full sertifisering og pålitelig levering. Vi tilbyr transparente priser uten skjulte avgifter og gir teknisk støtte gjennom hele anskaffelsesprosessen.
For gjeldende priser, tilgjengelighet eller teknisk konsultasjon, vennligstkontakt vårt salgsteam.